Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 93.0 MPa @Temperature -40.0 °C |
13500 psi @Temperature -40.0 °F |
ASTM D638 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 93.0 MPa @Temperature -40.0 °C |
13500 psi @Temperature -40.0 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 93.0 MPa @Temperature -40.0 °C |
13500 psi @Temperature -40.0 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |