Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 420 MPa @Diameter 105 - 200 mm |
60900 psi @Diameter 4.13 - 7.87 in |
|
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar .. |
|||
Tensile Strength | 420 MPa @Diameter 205 - 600 mm |
60900 psi @Diameter 8.07 - 23.6 in |
|
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar .. |
|||
Tensile Strength | 420 MPa @Thickness 152.4 - 203.2 mm |
60900 psi @Thickness 6.000 - 8.000 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength | 420 MPa @Thickness 203.2 - 254 mm |
60900 psi @Thickness 8.000 - 10.0 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength | 420 MPa @Thickness 5.90 - 15.0 mm |
60900 psi @Thickness 0.232 - 0.591 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |