Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 410 MPa @Thickness 450 - 700 mm |
>= 59500 psi @Thickness 17.7 - 27.6 in |
long-transverse direction |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Tensile Strength | >= 410 MPa @Thickness 450 - 700 mm |
>= 59500 psi @Thickness 17.7 - 27.6 in |
Temper T652 |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Tensile Strength | 410 MPa @Thickness 15.0 - 35.0 mm |
59500 psi @Thickness 0.591 - 1.38 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength | 410 MPa @Thickness 60.0 - 80.0 mm |
59500 psi @Thickness 2.36 - 3.15 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength | >= 410 MPa @Thickness 5.90 - 15.0 mm |
>= 59500 psi @Thickness 0.232 - 0.591 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |