Mechanical Properties Metric English Comments
Tensile Strength 210 MPa

@Diameter 80.0 - 150 mm
30500 psi

@Diameter 3.15 - 5.91 in
United Cast Bar Unibar 300 Continuously Cast Iron
Unibar 300 is alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and an excellent surface finish..
Tensile Strength >= 210 MPa

@Thickness 150 - 500 mm
>= 30500 psi

@Thickness 5.91 - 19.7 in
Temper 03
Constellium Alumold® 110 Aluminum Cast Sliced Plate
Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma..
Tensile Strength >= 210 MPa

@Thickness 500 - 600 mm
>= 30500 psi

@Thickness 19.7 - 23.6 in
Temper 03
Constellium Alumold® 110 Aluminum Cast Sliced Plate
Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma..
Tensile Strength >= 210 MPa

@Thickness 150 - 500 mm
>= 30500 psi

@Thickness 5.91 - 19.7 in
Temper O3
Constellium Fibral® Cast Aluminum Sliced Plate
Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia..
Tensile Strength >= 210 MPa

@Thickness 500 - 600 mm
>= 30500 psi

@Thickness 19.7 - 23.6 in
Temper O3
Constellium Fibral® Cast Aluminum Sliced Plate
Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia..
Tensile Strength 210 MPa

@Temperature -40.0 °C
30500 psi

@Temperature -40.0 °F
ASTM D638
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..