Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.0 MPa @Temperature 90.0 °C |
2900 psi @Temperature 194 °F |
ASTM D638 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 20.0 - 24.0 MPa @Temperature 75.0 °C |
2900 - 3480 psi @Temperature 167 °F |
|
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |
|||
Tensile Strength | 20.0 MPa @Strain 5.00 %, Temperature 100 °C |
2900 psi @Strain 5.00 %, Temperature 212 °F |
50mm/min |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Tensile Strength | 20.0 MPa @Strain 1.00 %, Temperature 60.0 °C |
2900 psi @Strain 1.00 %, Temperature 140 °F |
ISO 527 |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |