Mechanical Properties Metric English Comments
Modulus of Rupture 0.00207 GPa
0.300 ksi
De-aired, Extruded, 50% Kaolin/50% Flint
Imerys Allenâ„¢ G Kaolin
Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys
Modulus of Rupture 0.00207 GPa
0.300 ksi
Imerys EPK Kaolin
EPK Kaolin is a unique, high quality water washed ceramic kaolin which offers very white fired color, unusually good forming characteristics and high green strength. In glaze, EPK offers excellent s..
Modulus of Rupture 0.00207 GPa
0.300 ksi
Imerys Hamiltonâ„¢ Kaolin
Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit..
Modulus of Rupture 0.00207 GPa
0.300 ksi
dry
Imerys Kaolin Slurryâ„¢
Kaolin Slurry is a carefully controlled Kaolin-water suspension formulated for use in cermic castings.Information provided by Imerys
Modulus of Rupture 0.00207 GPa
0.300 ksi
parallel to thickness
Zircar Refractory Composites RS-99-45 Refractory Sheet
ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani..
Modulus of Rupture 0.00207 GPa
0.300 ksi
Green (typ.)
Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..