Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 28.1 GPa @Temperature 232 °C |
4080 ksi @Temperature 450 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement Laminate Physicals: 53% Fiber volume, 29% Resin content, 0.5% VoidsInformation provided by HexCel |
|||
Compressive Modulus | 28.1 GPa @Temperature 24.0 °C |
4080 ksi @Temperature 75.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |