Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 55.0 MPa @Temperature 200 °C |
7980 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 55.0 MPa @Temperature 200 °C |
7980 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Compressive Strength | 55.0 MPa @Temperature 200 °C |
7980 psi @Temperature 392 °F |
Result based on 450GL30; ISO 604 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Compressive Strength | 55.0 MPa @Temperature 200 °C |
7980 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Compressive Strength | 55.0 MPa @Temperature 250 °C |
7980 psi @Temperature 482 °F |
ISO 604 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Compressive Strength | 55.0 MPa @Temperature 250 °C |
7980 psi @Temperature 482 °F |
ISO 604 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 1300 °C |
7980 - 9430 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HC Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 110 °C |
7980 - 9430 psi @Temperature 230 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 1300 °C |
7980 - 9430 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 H Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc.. |
|||
Compressive Strength | 55.0 - 65.0 MPa @Temperature 100 °C |
7980 - 9430 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid.. |
|||
Compressive Strength | 55.0 MPa @Strain 1 % |
7980 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Compressive Strength | 55.0 MPa @Temperature 200 °C |
7980 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |