Mechanical Properties Metric English Comments
Compressive Strength 49.0 MPa

@Temperature 1095 °C
7110 psi

@Temperature 2003 °F
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable
Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode..
Compressive Strength 49.0 MPa

@Strain 2 %
7110 psi

@Strain 2 %
ISO 604
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data)
Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette..
Compressive Strength >= 49.0 MPa

@Temperature 1100 °C
>= 7110 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables
Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and ..
Compressive Strength 49.0 MPa

@Temperature 1500 °C
7110 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics REFCAST 80 High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 49.0 MPa

@Temperature 1500 °C
7110 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 49.0 MPa

@Temperature 110 °C
7110 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 49.0 MPa

@Temperature 110 °C
7110 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST SPECIAL Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Compressive Strength 49.0 MPa

@Temperature 1400 °C
7110 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-45 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 49.0 MPa

@Temperature 800 °C
7110 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-80 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 49.0 MPa

@Temperature 1400 °C
7110 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-Fused Silica Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 49.0 MPa

@Temperature 1500 °C
7110 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics REFCAST C High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 49.0 MPa

@Temperature 1000 °C,
Time 10800 sec
7110 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories BPCT-170 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 1500 °C,
Time 10800 sec
7110 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CTC-63TD Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 - 58.8 MPa

@Temperature 1500 °C,
Time 10800 sec
7110 - 8530 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HAPT-80S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 1500 °C,
Time 10800 sec
7110 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories joint-1 Blast Furnace Runner Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 110 °C,
Time 86400 sec
7110 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories LPCT-17PI Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 110 °C,
Time 86400 sec
7110 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SFC-60 SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 1350 °C,
Time 10800 sec
7110 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories TCH-175S Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 1350 °C,
Time 10800 sec
7110 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories TCH-175Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 49.0 MPa

@Temperature 1371 °C
7110 psi

@Temperature 2500 °F
Cold Crush Strength
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..
Compressive Strength 49.0 MPa

@Strain 2 %
7110 psi

@Strain 2 %
ISO 604
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data)
Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte..
Copyright © lookpolymers.com All Rights Reserved