Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 30.0 MPa @Strain 4.00 %, Temperature 23.0 °C |
4350 psi @Strain 4.00 %, Temperature 73.4 °F |
X direction, Condition A; ASTM D695 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Compressive Strength | 30.0 MPa @Temperature 200 °C |
4350 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 100 °C |
4350 - 5800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 110 C Dense Refractory Castable Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 100 °C |
4350 - 5800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 C Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 100 °C |
4350 - 5800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 1600 °C |
4350 - 5800 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 1000 °C |
4350 - 5800 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 1000 °C |
4350 - 5800 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 100 °C |
4350 - 5800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 GM Dense Refractory Castable Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro.. |
|||
Compressive Strength | 30.0 - 40.0 MPa @Temperature 1400 °C |
4350 - 5800 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan.. |
|||
Compressive Strength | 30.0 MPa @Temperature 200 °C |
4350 psi @Temperature 392 °F |
Result based on HT G22; ISO 604 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |