Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 290 MPa @Temperature 23.9 °C |
42000 psi @Temperature 75.0 °F |
Dry; CMC form; ASTM D695 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Compressive Strength | 290 MPa @Temperature 23.0 °C |
42100 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Compressive Strength | 290 MPa @Temperature 23.0 °C |
42100 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |