Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
Result based on 450GL30; ISO 604 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Compressive Strength | 250 MPa @Temperature 120 °C |
36300 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
Dry; EN2850B |
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ.. |
|||
Compressive Strength | 250 MPa @Temperature 120 °C |
36300 psi @Temperature 248 °F |
Dry; EN2850B |
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ.. |
|||
Compressive Strength | 250 MPa @Temperature 200 °C |
36300 psi @Temperature 392 °F |
|
Elisto THERMOSTAR® 600 n Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Compressive Strength | 250 MPa @Temperature 200 °C |
36300 psi @Temperature 392 °F |
|
Elisto THERMOSTAR® LC 400 GL Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Compressive Strength | 250 MPa @Temperature 23.0 °C |
36300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |