Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 163 GPa @Temperature -67.0 °C |
23700 ksi @Temperature -88.6 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Tensile Modulus | 163 GPa @Temperature 220 °C |
23700 ksi @Temperature 428 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Tensile Modulus | 163.4 GPa @Temperature 232 °C |
23700 ksi @Temperature 450 °F |
IM7 (12K); [0°]8 |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |