Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.80 GPa @Temperature 23.0 °C |
1130 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Tensile Modulus | 7.80 GPa @Temperature 23.0 °C |
1130 ksi @Temperature 73.4 °F |
|
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Tensile Modulus | 7.80 GPa @Temperature 60.0 °C |
1130 ksi @Temperature 140 °F |
|
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Tensile Modulus | 7.80 GPa @Temperature 60.0 °C |
1130 ksi @Temperature 140 °F |
|
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Tensile Modulus | 7.80 GPa @Temperature 120 °C |
1130 ksi @Temperature 248 °F |
|
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Tensile Modulus | 7.80 GPa @Temperature 60.0 °C |
1130 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 7.80 GPa @Temperature 23.0 °C |
1130 ksi @Temperature 73.4 °F |
|
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Metal stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE freeAvailability: A.. |
|||
Tensile Modulus | 7.80 GPa @Temperature 23.0 °C |
1130 ksi @Temperature 73.4 °F |
|
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 7.80 GPa @Temperature 60.0 °C |
1130 ksi @Temperature 140 °F |
|
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |