Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 64.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 64.8 GPa

@Temperature 121 °C
9400 ksi

@Temperature 250 °F
0° Direction, Dry, 365° Oven Cured; ASTM D3039
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Tensile Modulus 64.8 GPa

@Temperature 121 °C
9400 ksi

@Temperature 250 °F
0° Direction, Wet, 365° Oven Cured; ASTM D3039
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Tensile Modulus 64.8 GPa

@Temperature 19.4 °C
9400 ksi

@Temperature 67.0 °F
CTD, 90° Direction; SACMA SRM 4R-94
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Tensile Modulus 64.8 GPa

@Temperature -55.0 °C
9400 ksi

@Temperature -67.0 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric
Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel
Tensile Modulus 64.8 GPa

@Temperature -59.0 °C
9400 ksi

@Temperature -74.2 °F
T300, Plain Weave; Fill Tension;
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form
Fiber: T300-3KInformation provided by HexCel
Tensile Modulus 64.8 GPa

@Temperature 200 °C
9400 ksi

@Temperature 392 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel
Copyright © lookpolymers.com All Rights Reserved