Mechanical Properties Metric English Comments
Tensile Modulus 11.7 GPa

@Temperature 23.0 °C
1700 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)
Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also..
Tensile Modulus 11.7 GPa

@Temperature 90.0 °C
1700 ksi

@Temperature 194 °F
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Carbon fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
Tensile Modulus 11.7 GPa

@Temperature 77.0 °C
1700 ksi

@Temperature 171 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Information provided by HexCel