Mechanical Properties Metric English Comments
Tensile Modulus 1.25 GPa

@Temperature 60.0 °C
181 ksi

@Temperature 140 °F
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 1.25 GPa

@Temperature 23.0 °C
181 ksi

@Temperature 73.4 °F
1 mm/min; ISO 527-2
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r..