Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.900 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.900 GPa

@Temperature 120 °C
131 ksi

@Temperature 248 °F
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 0.900 GPa

@Temperature 60.0 °C
131 ksi

@Temperature 140 °F
LATI Latan 13E71 POM
Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided ..
Tensile Modulus 0.900 GPa

@Temperature 90.0 °C
131 ksi

@Temperature 194 °F
LATI Latan 9 POM
Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Tensile Modulus 0.900 GPa

@Temperature 23.0 °C
131 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
Tensile Modulus 0.900 GPa

@Temperature 23.0 °C
131 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
Tensile Modulus 0.900 GPa

@Temperature 100 °C
131 ksi

@Temperature 212 °F
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Tensile Modulus 0.900 GPa

@Temperature 23.0 °C
131 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
Tensile Modulus 0.900 GPa

@Temperature 60.0 °C
131 ksi

@Temperature 140 °F
LATI Later 4 PBT
Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.