Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 45.0 MPa @Temperature 23.0 °C |
6530 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D638 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 45.0 MPa @Temperature 80.0 °C |
6530 psi @Temperature 176 °F |
Practical Use (Water Absorption 2.1%); ASTM-D638 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 45.0 MPa @Temperature 23.0 °C |
6530 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.0%); ASTM-D638 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 45.0 MPa @Temperature 23.0 °C |
6530 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 3.5%); ASTM-D638 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 45.0 MPa @Temperature 80.0 °C |
6530 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 45.0 MPa @Temperature -40.0 °C |
6530 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.0%); ASTM-D638 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |