Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.0 MPa @Temperature 100 °C |
4930 psi @Temperature 212 °F |
X direction, Condition A; ASTM D638 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 100 °C |
4930 psi @Temperature 212 °F |
Y direction, Condition A; ASTM D638 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Tensile Strength, Ultimate | 34.0 MPa @Temperature 23.0 °C |
4930 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D638 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |