Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 115 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa

@Temperature 980 °C
16700 psi

@Temperature 1800 °F
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Tensile Strength, Ultimate 115 MPa

@Temperature 1000 °C
16700 psi

@Temperature 1830 °F
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Ultimate 115 MPa

@Temperature -40.0 °C
16700 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.3%); ASTM-D638
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 115 MPa

@Temperature 23.0 °C
16700 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.7%); ASTM-D638
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 115 MPa

@Temperature 80.0 °C
16700 psi

@Temperature 176 °F
Practical Use (Water Absorption 1.25%); ASTM-D638
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 115 MPa

@Temperature -40.0 °C
16700 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 115 MPa

@Temperature 23.0 °C
16700 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.6%); ASTM-D638
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 115 MPa

@Temperature 1000 °C
16700 psi

@Temperature 1830 °F
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Copyright © lookpolymers.com All Rights Reserved