Polymer Property : Peel Strength = 90.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 15.8 kN/m
90.0 pli
180°, PVC, Cotton duck failed during testing
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 15.8 kN/m
90.0 pli
180°, Polycarbonate, Cotton duck failed during testing
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 15.8 kN/m
90.0 pli
180°, PVC, Cotton duck failed during testing
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 15.8 kN/m
90.0 pli
180°, FRP, Cotton duck failed during testing
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 15.8 kN/m
90.0 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..