Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.8108 kN/m | 4.625 pli | Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9505 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9671LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Faceside, to Stainless Steel, 180° Peel, 2 mil Al |
3M XR8123 Double Coated Paper Tapes 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 8132LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Polypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330 |
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9552 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 90°, 72 hr RT; ASTM D3330 |
3M 9828HL Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330 |
3M 9555 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | ABS, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330 |
3M 9731 Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Peel Strength | 0.8108 kN/m | 4.625 pli | ABS, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330 |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |