Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.53686 kN/m | 3.0625 pli | Adhesion to Steel, 90° Peel, 5 in/min, Initial; ASTM D3330 |
3M 253 Silicone Splicing Tape 3M™ Sealing Splicing Tape 253 is a single-coated paper tape with a modified poly liner implemented as a second liner on the FACE SIDE of the tape. This second liner is added to help ensure roll qua.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Stainless Steel, 90°, 15 min RT; ASTM D3330 |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Smooth Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | 90° Peel, PET/PET, Initial (20 mins); ASTM D3330 |
3M 7945MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Stainless Steel, 90°, 15 min RT, Faceside; ASTM D3330 |
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.53686 kN/m | 3.0625 pli | 90° Peel, PET/PET, Initial (20 mins); ASTM D3330 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |