Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.38 kN/m | 25.0 pli | Tensile |
Dielectric Polymers NT-711 Electrical/Mechanical Tape
(discontinued **) High temperature acrylic adhesive with polyester film backing.Features: High temperature shear propertiesSolvent resistantTemperature class: 266°FInsulation resistance: > 1x106 M?Electrolytic corro.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | T-peel |
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 180°, Canvas to aluminum, pulled at 2"/min |
3M Scotch-Seal™ 2084 Metal Sealant Features: 3M™ Scotch-Seal™ Metal Sealant 2084 is a one-part aluminum colored sealant which air dries to a tough, flexible film that resists water, oils and fuel. Retains sealing properties after e.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M SJ5300 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polypropylene |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polypropylene |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Polystyrene |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | Bond Strength; ASTM D624 |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | T-Peel |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | T-Peel |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | T-Peel |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Peel Strength | 4.38 kN/m | 25.0 pli | CRS, T-Peel, 17-20 mil bondline, MEK/abrade/MEK |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |