Polymer Property : Peel Strength = 2.28 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.28 kN/m
13.0 pli
ASTM D903
Permabond 738 Cyanoacrylate, toughened
PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over..
Peel Strength 2.28 kN/m
13.0 pli
Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic
Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED).
Peel Strength 2.28 kN/m
13.0 pli
on canvas
3M Scotch-Weld™ 3792LM Low Melt Adhesive
Clear multi-purpose for wood, coated paper, polyolefins and other heat-sensitive materials; P.O.P. displays and use with low melt applicator onlyInformation provided by 3M
Peel Strength 2.28 kN/m
13.0 pli
180°
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..
Peel Strength 2.28 kN/m
13.0 pli
180°, Polyacrylic
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 2.28 kN/m
13.0 pli
on canvas
3M Scotch-Weld™ 3792 Hot Melt Adhesive
Clear, multi-purpose for wood, corrugated, fabric, fur nature, upholstery, novelties, and other lightweight materialsInformation provided by 3M
Peel Strength 2.28 kN/m
13.0 pli
Aluminum-Supported Vinyl, 180°, Aging 7 Day @ 140°F
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
Peel Strength 2.28 kN/m
13.0 pli
Polyester-Supported Vinyl, 180°, Aging 7 Day @ 100% RH
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
Peel Strength 2.28 kN/m
13.0 pli
on canvas
3M Scotch-Weld™ 3738 Hot Melt Adhesive
High delivery rate and long bonding rage and General purpose for foundry san cores, wood bonding, corrugated, selected plastics and chipboardInformation provided by 3M
Peel Strength 2.28 kN/m
13.0 pli
on canvas
3M Scotch-Weld™ 3755LM Low Melt Adhesive
“Delayed-tack” applied in thin-glue-line ribbon for paper, corrugated, chipboard, displays, exhibits and Use with low melt applicator onlyInformation provided by 3M