Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
Water Absorption 0.020 %
0.020 %
Mechanical Properties Metric English Comments
Peel Strength 2.28 kN/m
13.0 pli
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
x direction
12.0 µm/m-°C
6.67 µin/in-°F
y direction
CTE, linear, Transverse to Flow 125 µm/m-°C
69.4 µin/in-°F
z direction
Thermal Conductivity 0.320 W/m-K
2.22 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.0

@Frequency 1.00e+10 Hz
3.0

@Frequency 1.00e+10 Hz
3.0

@Thickness 0.508 mm
3.0

@Thickness 0.0200 in
3.0

@Thickness 3.17 mm
3.0

@Thickness 0.125 in
Dissipation Factor 0.0020

@Frequency 1.00e+10 Hz
0.0020

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -110