Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.9861 kN/m | 5.625 pli | Adhesion to Steel; ASTM D3330 |
3M 33803 General Purpose Aluminum Foil Tape High tack rubber adhesive. 40 lb liner. UL 723 ClassifiedInformation provided by 3M |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Rigid PVC, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485PC Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Glass, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9482PC Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 720 Film/Fiber Tape Scotch® Tape 720 is a semi-transparent tape featuring a high tack, aggressive adhesive and a hand tearable film/fiber backing. It can be used for general purpose sealing and attaching, especially u.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Adhesion to Steel; ASTM D3330 |
3M 3311 General Purpose Aluminum Foil Tape Ul 723 listedInformation provided by 3M |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Stainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 8153LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Glass, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9442 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Rigid PVC, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9445 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330 |
3M 9475LE High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Faceside; ASTM D3330 |
3M 9475LE High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330 |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Faceside; ASTM D3330 |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | ABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330 |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | LDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9627 Adhesive Transfer Tape with Quick Bonding Adhesive 360 3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polypropylene, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | ABS, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Polypropylene, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | ABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | ABS, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Stainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9653LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 0.9861 kN/m | 5.625 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 3311 Foil Tape Scotch® Foil Tape 3311 is an aluminum alloy foil with a pressure-sensitive adhesive and paper liner. The aggressive rubber adhesive sticks well to most surfaces and the paper liner makes for conven.. |