Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.877 kN/m | 5.00 pli | Copper, After Solder Float, 1/2 ounce TCR Foil; IPC-TM-650 2.4.8 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Peel Strength | 0.877 - 3.51 kN/m | 5.00 - 20.0 pli | Average value: 2.48 kN/m Grade Count:6 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | After Thermal Stress; IPC TM-650 2.4.8 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP032708 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are clear materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tac.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-37 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-41 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-46 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-77 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Alodine, aluminum |
3M Scotchcal™ 50-745 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-24 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-27 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7725-12 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7725-193 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7725-197 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | 72 hour RT glass, 90° peel, 2 mil aluminum foil backing |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Polypropylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9445 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.877 - 1.05 kN/m | 5.00 - 6.00 pli | Adhesion to Aluminum, etched |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-197 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Alodine, aluminum |
3M Scotchcal™ 50-78 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-38 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-54 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-58 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7725-49 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM04190E White Polyester Label Products 3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which .. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ 1000-22 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
3M Scotchcal™ ElectroCut™ 7125-88 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
Arlon 44560R009W 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, .. |