Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.71216 kN/m | 4.0625 pli | 24 hr, Non-linered side-Photopolymer; ASTM D3330 |
3M 2205 Thin Flexographic Plate Mounting Tape 3M™ Thin Flexographic Mounting Tape 2205 is a double coated film tape constructed of a polyester film carrier with differential adhesives specifically designed for the corrugated printing business .. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | 72 hour RT polycarbonate, 90° peel, 5 mil aluminum foil backing |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1020R Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1040 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1040 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1815M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1815M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1015 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Urethane-B, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1020 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1060H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1520 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1840H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | ABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330 |
3M 9552 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Polypropylene, 180°, 2 mil al foil, 15 min RT, Backside; ASTM D3330 |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1920S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8886 Stretchable Tape Scotch® Stretchable Tape is a high performance transparent stretchable tape, designed to contain A- and B- pallets for internal and external shipping purposes.Information provided by 3M |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | 72 hour RT polycarbonate, 90° peel, 5 mil aluminum foil backing |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | 72 hour RT polycarbonate, 90° peel, 5 mil aluminum foil backing |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Adhesion to Anodized Aluminum, after 7 days in water; ASTM D3330 |
3M 8067 All Weather Flashing Tape 3M™ All Weather Flashing Tape 8067 is a self-adhered, waterproof flashing membrane designed for sealing around openings and penetrations in exterior walls. This product has a unique acrylic pressur.. |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | LDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | LDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.71216 kN/m | 4.0625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1920M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |