Polymer Property : Peel Strength = 0.42729 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
3M 7014 Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
3M 7014FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7600 Removable Vinyl Label Material
3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7744FL Polyester Overlaminating Film
3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7745FL Polyester Overlaminating Film
3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r..
Peel Strength 0.42729 kN/m
2.4375 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7779 Polypropylene Label Material
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating..
Peel Strength 0.42729 kN/m
2.4375 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7850TL Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for..
Peel Strength 0.42729 kN/m
2.4375 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7850TL Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for..
Peel Strength 0.42729 kN/m
2.4375 pli
to Steel; ASTM D3330
3M Scotch® 2380 Performance Masking Tape
Scotch® Performance Masking Tape 2380 is a smooth, strong, mini-crepe paper masking tape suitable for most paint masking applications.Information provided by 3M
Peel Strength 0.42729 kN/m
2.4375 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7011 Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.42729 kN/m
2.4375 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7011FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
3M 7014FL Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7200 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate..
Peel Strength 0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7901 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7920 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive ..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7744 Polyester Overlaminating Film
3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l..
Peel Strength 0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7884 White Vinyl Label Material
Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7902 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate..
Peel Strength 0.42729 kN/m
2.4375 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7906 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate..
Peel Strength 0.42729 kN/m
2.4375 pli
90° Peel, PET/PET, Initial (20 mins); ASTM D3330
3M 7997MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Peel Strength 0.42729 kN/m
2.4375 pli
ABS, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330
3M 9731 Double Coated Tape
3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other ..
Peel Strength 0.42729 kN/m
2.4375 pli
ABS, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330
3M 9731RW Double Coated Tape
3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other ..