Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.27391 kN/m | 1.5625 pli | Composite Sleeve, Adhesion; ASTM D3330 |
3M 413DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | to Steel; ASTM D3330 |
3M 465 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330 |
3M 665 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7002FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7735FL Acrylate Overlaminating Film 3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers exc.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | to Steel; ASTM D3330 |
3M 9420 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | to Steel; ASTM D3330 |
3M 9457 Adhesive Transfer Tape with 3M Adhesive 400 3M™ Adhesive Transfer Tapes 463, 465, 9457 and 9665 with 3M™ Adhesive 400 are ideal for bonding together a wide variety of similar and dissimilar materials such as metals, glass, wood, papers, pai.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1015 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1120 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1315 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 415 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 4193-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4193-EZ is an easy (EZ) unwind polyethylene tape with a very high-tack adhesive system.Information provided by 3M |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Adhesion to Housewrap; ASTM D3330 |
3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1815 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1920S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1320 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.27391 kN/m | 1.5625 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |