Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.1205 kN/m | 0.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 25X187 Protective UV Tape 3M™ Protective UV Tape 25X187 is a black and white co-extruded polyethylene tape featuring limited UV resistance.Information provided by 3M |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 3187 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3187 has a high-tack adhesive system to help provide temporary protection of many textured metals, plastics and molded fiberglass materials with minimum adhesion b.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7002 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7002FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Layer-to-Layer Adhesion; ASTM D3330 |
3M Scotchgard™ 1002 Multi-Layer Protective Films 3M™ Scotchgard™ Multi-Layer Protective Films 1002 is optically transparent, pressure-sensitive polyester film tapes designed to protect surfaces from intentional and unintentional damage caused by.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Layer-to-Layer Adhesion; ASTM D3330 |
3M Scotchgard™ 1004 Multi-Layer Protective Films 3M™ Scotchgard™ Multi-Layer Protective Films 1004 is optically transparent, pressure-sensitive polyester film tapes designed to protect surfaces from intentional and unintentional damage caused by.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 4H83C Protective Laser Tape 3M™ Protective Laser Tape 4H83 is a clear or white multi-polymer film coated with medium-tack adhesive designed especially to help provide temporary protection of #3 & #4 stainless steel sheets dur.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 4H83W Protective Laser Tape 3M™ Protective Laser Tape 4H83 is a clear or white multi-polymer film coated with medium-tack adhesive designed especially to help provide temporary protection of #3 & #4 stainless steel sheets dur.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7011 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.1205 kN/m | 0.6875 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |