Mechanical Properties Metric English Comments
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene
ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009..
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade
PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requir..
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe..
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
ExxonMobil LD 117.85 Blown Overwrap Film Resin
Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac..
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin
Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac..
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl..
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)
Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus..
Copyright © lookpolymers.com All Rights Reserved