Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM D882 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatu.. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM D882 |
Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties .. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM D882 |
Braskem Green PE SLL218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL218 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for cast film extrusion. Films obtained with this product show a good processing performance balanced with .. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM-D882 |
Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer LF 118/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prop.. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM-D882 |
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p.. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM-D882 |
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin.. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM D882 |
Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene Description: LL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties a.. |
|||
1% Secant Modulus, TD | 230 MPa | 33400 psi | ASTM D882 |
Braskem LL218 Cast Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |