Mechanical Properties Metric English Comments
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Westlake EB561 6.5% Ethylene Vinyl Acetate Copolymer  (discontinued **)
Excellent sealability, excellent impact strength, good optics and enhanced stabilization.Application/UsesFrozen food packagingFresh food packagingIce bagsHeavy duty produce bagsFDA: This material co..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Westlake Elevate™ EF561 6.5% Ethylene Vinyl Acetate Copolymer
Westlake EF 561 resin is a fractional melt index 6.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. T..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Westlake Elevate™ EF575 7.5% Ethylene Vinyl Acetate Copolymer
Westlake EF 575 resin is a fractional melt index 7.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. T..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Westlake Elevate™ EF598 9% Ethylene Vinyl Acetate Copolymer
Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer
Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, ..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applica..
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
ExxonMobil Escorene™ FL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00112 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No App..
Copyright © lookpolymers.com All Rights Reserved