Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009.. |
|||
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requir.. |
|||
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe.. |
|||
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
ExxonMobil LD 117.85 Blown Overwrap Film Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |
|||
1% Secant Modulus, TD | 379 MPa | 55000 psi | ASTM D882 |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |