Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 241 MPa | 34900 psi | ASTM D882 |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D638 |
LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake EF418 Low Density Polyethylene WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake EN1817AA Low Density Polyethylene Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake EN1820 Low Density Polyethylene Westlake Polyethylene EN1820 natural is a low density formulation with outstanding optical properties, making this material an excellent choice for calendaring and as a clarity filler in coextruded .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake Hifor LT74104 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74104 is a high strength linear low density polyethylene containing no slip or antiblock. It is designed for blown film applications and is well suited for consumer an.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake Hifor LT74105 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74105 is a high strength linear low density polyethylene containing medium slip and medium antiblock. It is designed for blown film applications and is well suited for.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake Hifor LT74113 Hexene Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74113 is a high strength hexene linear low density polyethylene containing no slip and medium antiblock. It is designed for blown film applications and is well suited .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake Hifor LT74119 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74119 is a high strength linear low density polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applic.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
Westlake Hifor LT74147 Linear Low Density Polyethylene WESTLAKE HIFOR Polyethylene LT74147 is a high strength linear low density polyethylene containing medium slip and high antiblock. It is designed for blown film applications and is well suited for c.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05HH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Exceed™ 1023JA Metallocene Polyethylene Resin Product Description: Exceed 1023JA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1023JA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil LD 051.LQ Shrink Film Resin L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 241 MPa | 35000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |