Polymer Property : 1% Secant Modulus, MD = 34000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
Westlake EB169 Low Density Polyethylene
Westlake EB169 is a low-density polyethylene with high stiffness designed for beverage shrink overwrap and towel/tissue packaging. It has good toughness and blends well with LLDPE resins.Application..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
Westlake Hifor Clear SC74558 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74558 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives...
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LD 071.LQ Blown Film Resin
L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LD 071.LR Blown Film Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LD 124.MS General Purpose Clarity Film Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..