Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, MD = 170 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 170 MPa
24700 psi
ISO 527-3
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene
Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH ..
1% Secant Modulus, MD 170 MPa
24700 psi
ISO 527-3
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta..
1% Secant Modulus, MD 170 MPa
24700 psi
ISO 527-3
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM D 882
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin
PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM D 882
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin
PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM-D882
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer
The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM-D882
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer
LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM D882
Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene
Description: LH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount.Applications: Lamina..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM D882
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas..
1% Secant Modulus, MD 170 MPa
24700 psi
ASTM-D882
Braskem LF218/21 LLDPE Cast and Blown Film Extrusion Polyethylene Copolymer
LF218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prope..
Copyright © lookpolymers.com All Rights Reserved