Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 42.0 - 260 MPa @Temperature -40.0 - 150 °C |
6090 - 37700 psi @Temperature -40.0 - 302 °F |
Average value: 109 MPa Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 42.0 - 260 MPa @Thickness 0.800 - 3.17 mm |
6090 - 37700 psi @Thickness 0.0315 - 0.125 in |
Average value: 109 MPa Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 68.9 - 260 MPa | 10000 - 37700 psi | Average value: 139 MPa Grade Count:37 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Flexural Yield Strength | 240 - 260 MPa @Temperature 80.0 - 80.0 °C |
34800 - 37700 psi @Temperature 176 - 176 °F |
Average value: 253 MPa Grade Count:4 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Flexural Yield Strength | 11.5 - 260 MPa | 1670 - 37700 psi | Average value: 172 MPa Grade Count:193 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Flexural Yield Strength | 90.0 - 260 MPa | 13100 - 37700 psi | Average value: 176 MPa Grade Count:91 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 110 - 260 MPa | 16000 - 37700 psi | Average value: 177 MPa Grade Count:43 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |