Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 66.7 MPa | 9670 psi | ASTM D790 |
Samsung Cheil Industries Starex® SD-0150 ABS, Unreinforced
(discontinued **) Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: General Purpose: Good Impact Strength, Chemical Resistance, ProcessabilityApplications: Household Appliances, Auto Interior Trim and P.. |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 3.20 mm |
9670 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Flexural Yield Strength | 66.7 MPa @Thickness 6.40 mm |
9670 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |