Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 43.1 MPa | 6260 psi | ASTM D790 |
IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% BARIUM SULPHATE REINFORCED HIGH GLOSS APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES |
|||
Flexural Yield Strength | 43.1 MPa | 6260 psi | ASTM D790 |
IRPC Polimaxx Polene 2311LCX TA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Flexural Yield Strength | 43.2 MPa | 6260 psi | ASTM D790 |
KKPC Kuhmo HF400 Flame Retarded General Purpose HIPS Key features: Translucent Injection. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resista.. |
|||
Flexural Yield Strength | 43.1 MPa @Thickness 6.40 mm |
6260 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 43.1 MPa @Thickness 6.40 mm |
6260 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Flexural Yield Strength | 43.2 MPa | 6260 psi | ASTM D790 |
Devcon HVAC Repair (Special F) Epoxy General Repair EpoxyComments: Aluminum-filled epoxy adhesive, conveniently packaged in two 6.5 oz. tubes. Bonds to aluminum and other metals, ceramics, wood, concrete or glass. Use as an adhesive .. |