Polymer Property : Flexural Yield Strength = 207 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 24.1 - 207 MPa
3500 - 30000 psi
Average value: 150 MPa Grade Count:55
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Flexural Yield Strength 85.0 - 207 MPa
12300 - 30000 psi
Average value: 151 MPa Grade Count:37
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Flexural Yield Strength 93.1 - 207 MPa
13500 - 30000 psi
Average value: 142 MPa Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Flexural Yield Strength 10.0 - 207 MPa
1450 - 30000 psi
Average value: 52.0 MPa Grade Count:48
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Flexural Yield Strength 25.0 - 207 MPa

@Temperature -40.0 - 120 °C
3630 - 30000 psi

@Temperature -40.0 - 248 °F
Average value: 84.2 MPa Grade Count:6
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Flexural Yield Strength 58.6 - 207 MPa
8500 - 30000 psi
Average value: 130 MPa Grade Count:89
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Flexural Yield Strength 75.8 - 207 MPa
11000 - 30000 psi
Average value: 130 MPa Grade Count:47
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Yield Strength 128 - 207 MPa
18500 - 30000 psi
Average value: 169 MPa Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..
Flexural Yield Strength 103 - 207 MPa
15000 - 30000 psi
Average value: 153 MPa Grade Count:10
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Flexural Yield Strength 83.0 - 207 MPa
12000 - 30000 psi
Average value: 158 MPa Grade Count:21
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Flexural Yield Strength 77.9 - 207 MPa
11300 - 30000 psi
Average value: 109 MPa Grade Count:37
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved