Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 86.3 MPa @Thickness 3.20 mm |
12500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 86.3 MPa @Thickness 6.40 mm |
12500 psi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Flexural Yield Strength | 86.3 MPa @Thickness 3.20 mm |
12500 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 86.3 MPa @Thickness 3.20 mm |
12500 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 86.3 MPa @Thickness 3.20 mm |
12500 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY NS5000 PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 86.3 MPa | 12500 psi | ASTM D790 |
Samyang Trirex® 3022A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 86.3 MPa | 12500 psi | ASTM D790 |
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 86.3 MPa | 12500 psi | ASTM D790 |
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 86.3 MPa | 12500 psi | ASTM D790 |
Samyang Trirex® 3026PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 86.3 MPa | 12500 psi | ASTM D790 |
Samyang Trirex® 3025A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 86.3 MPa | 12500 psi | ASTM D790 |
Samyang Trirex® 3026B Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026B is an extrusion grade.Applications: BottlesInformation provided by Samyang. |