Polymer Property : Flexural Yield Strength = 229 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 229 MPa
33200 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12
LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant.
Flexural Yield Strength 229 MPa
33200 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66
LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant.
Flexural Yield Strength 229 MPa
33200 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DE006 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE006 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Yield Strength 229 MPa
33200 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber.
Flexural Yield Strength 229 MPa
33200 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 9X11427
LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G..