Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 228 MPa | 33100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Flexural Yield Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Flexural Yield Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill® PPA GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu.. |
|||
Flexural Yield Strength | 228 MPa | 33000 psi | ASTM D790 |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 228 MPa | 33000 psi | ASTM D790 |
Clariant Renol 6608G33HSL Nylon 66, 33% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | ASTM D790 |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 228 MPa | 33100 psi | ASTM D790 |
Chem Polymer Durlex 740-10 GB PBT, 40% Short Glass Fiber, 10% Glass Bead Reinforced A 40% short glass fiber, 10% glass bead reinforced PBT, offering a combination of tensile strength, warpage control and dimensional stability for close tolerance applications.Data provided by the ma.. |