Polymer Property : Film Tensile Strength at Break, TD = 7000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 34.5 - 48.3 MPa
5000 - 7000 psi
ASTM D882
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, TD 34.5 - 48.3 MPa
5000 - 7000 psi
ASTM D882
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Film Tensile Strength at Break, TD 37.9 - 48.3 MPa
5500 - 7000 psi
ASTM D882
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film
Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag..
Film Tensile Strength at Break, TD 27.6 - 48.3 MPa
4000 - 7000 psi
ASTM D882
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..