Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Film Tensile Strength at Break, TD | 26.9 - 39.3 MPa | 3900 - 5700 psi | ASTM D882 |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LD 317.09 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LD 317.87 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Film Tensile Strength at Break, TD | 26.9 MPa | 3900 psi | ASTM D882 |
Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,.. |