Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop Test = 120 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I..
Dart Drop Test 120 g
0.265 lb
(method A); ASTM D1709
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating
The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene
Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the ..
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Polimeri Europa Flexirene® FG 23 F Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 23 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 F represents the version of Flexirene FG 20 F..
Dart Drop Test 120 g
0.265 lb
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Dart Drop Test 120 g
0.265 lb
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Dart Drop Test 120 g
0.265 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA960000 Low Density Polyethylene
ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif..
Dart Drop Test 120 g
0.265 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA960070 Low Density Polyethylene
ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un..
Dart Drop Test 120 g
0.265 lb
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA960083 Low Density Polyethylene
ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un..
Dart Drop Test 120 g
0.265 lb
ASTM D1709
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene
LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industria..
Dart Drop Test 120 g
0.265 lb
F<sub>50</sub>; ASTM D1709A
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Dart Drop Test 120 g
0.265 lb
ASTM D1709
SIDPEC EGYPTENE® HD 4602 FA HDPE Film
Applications:Strong filmTrash bagShopping bagFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official dis..
Dart Drop Test 120 g
0.265 lb
ISO 7765-1
Borealis FT5230 Low Density Polyethylene
FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: ..
Dart Drop Test 120 g

@Thickness 0.0400 mm
0.265 lb

@Thickness 0.00157 in
ISO 7765-1
Borealis FT5231 Low Density Polyethylene
FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d..
Dart Drop Test 120 g
0.265 lb
26 in; ASTM D1709
Chevron Phillips MarFlex® D350 m-LLDPE Linear Low Density Polyethylene
Low Density PolyethyleneCustomer Benefits: This medium density metallocene polyethylene film resins combines the benefits of .933 density (modulus, barrier, c.o.f.) with the clarity of mLLDPE.Applic..
Dart Drop Test 120 g
0.265 lb
ASTM D1709A
ExxonMobil EXACT™ 4053 Cast Plastomer
Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly..
Dart Drop Test 120 g
0.265 lb
ASTM D1709
ExxonMobil LD 316.19 High Clarity, High Impact Film Resin
LD 316.19 has improved impact strength and heat sealability versus homopolymer clarity film resins. Applications include frozen and other food packaging, as well as profile extrusion.Information pr..
Dart Drop Test 120 g
0.265 lb
ASTM-D1709
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene
CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE ..
Dart Drop Test 120 g
0.265 lb
ASTM-D1709
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer
The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I..
Dart Drop Test 120 g
0.265 lb
50.8 microns, Blown Film; ASTM D1709A
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
OverviewHigh melt strengthHigh toughnessExcellent processabilityHigh impact and puncture resistanceHigh film stiffness/machinabilityHigh heat resistanceComplies with U.S. FDA FCN 843, Europe EU-Dire..
Dart Drop Test 120 g
0.265 lb
gF/50%f; ASTM D1709
Braskem TS9022 Blown Film Extrusion Low Density Polyethylene
Films for automatic overwrap packaging of hygiene markets. Typical applications are toilet tissue, kitchen paper and napkin (paper product) overwrap. Films which require good optical properties al..
Dart Drop Test 120 g
0.265 lb
g/F50; ASTM D1709
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process..
Dart Drop Test 120 g
0.265 lb
ASTM-D1709
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene
TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad..
Dart Drop Test 120 g
0.265 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..
Dart Drop Test 120 g
0.265 lb
ASTM D1709
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin..
Copyright © lookpolymers.com All Rights Reserved